Chromium-silicon alloy targets are high-purity sputtering targets based on chromium (Cr) and silicon (Si) as core constituents, designed for magnetron sputtering and other physical vapor deposition (PVD) processes to deposit Cr-Si functional thin films onto substrates. Unlike stoichiometrically fixed chromium silicide compounds (such as CrSi₂), the essential characteristic of Cr-Si alloy targets lies in their tunable composition—continuous variation of the Cr/Si ratio endows the deposited films with a designable spectrum of properties ranging from electrical resistivity and temperature coefficient of resistance (TCR) to optical constants. This feature gives them a distinctive position in precision thin-film resistors, optical coatings, and sensor functional layers.
I. Composition System
The compositional design of Cr-Si alloy targets is not a single fixed value but is adjusted over a broad range according to application requirements. According to data disclosed in patent literature, the Cr-Si binary system covers a considerably wide compositional range: from Cr 70 at%/Si 30 at% to Cr 20 at%/Si 80 at%. Different composition ranges correspond to markedly different material behaviors and application scenarios.
In patents oriented toward structural components and conventional sputtering applications, a more commonly specified composition window is Si 1–30 at%, with the balance being Cr. This restriction has practical process considerations: when silicon content exceeds 30 at%, the brittleness of the target increases significantly, making it highly prone to cracking during sintering and subsequent machining, which sharply reduces yield. In other words, although high-silicon Cr-Si targets are attractive for certain optical applications, they impose more demanding requirements on the manufacturing process.
Beyond the binary system, multi-element microalloying represents another compositional design direction. One patent proposes incorporating 1–10 at% of one or more elements selected from B, Nb, W, Mo, Ta, or V into the Cr-Si base to form CrSiMe alloy targets. The purpose of such additions is typically to further tailor the microstructure or specific functionality of the film, though mainstream commercial products remain predominantly binary Cr-Si systems.
In terms of purity, metallic impurity control for high-end Cr-Si targets is generally above 99.9% to 99.95%. For precision resistor and semiconductor-related applications, control of interstitial impurities such as oxygen and carbon is equally critical, since these impurities can form scattering centers or trap charge carriers, degrading the electrical stability of the films.
II. Production Process
The core contradiction in the preparation of Cr-Si targets lies in the significant differences in physical properties between chromium and silicon, combined with the hard and brittle nature of high-silicon bodies that makes them prone to cracking. Industrial practice has developed multiple technical routes centered on powder metallurgy to address this challenge.
The conventional powder sintering route typically includes mixing, pre-sintering, pressing, and final sintering. Taking one patent embodiment as an example: chromium powder (purity 99.95%, average particle size 150 μm) and silicon powder (purity 99.9995%, average particle size 40 μm) are ball-milled at a mass ratio of 3:2 for 36 hours to obtain a mixed powder. The powder is then loaded into a mold, compacted, evacuated, and heated at 6.5 °C/min to 625 °C for a first pre-sintering hold of 1.5 hours, then at 3 °C/min to 900 °C for a second pre-sintering stage; subsequently, pressure is increased at 0.4 MPa/min to 28 MPa for a first pressing hold of 0.6 hours. After trimming, the pre-sintered compact enters a higher-temperature sintering and pressing stage: heating at a similar rate to 850–1100 °C for a first sintering, then to 1150–1350 °C for a second sintering, and finally pressing at 25–40 MPa for a second pressing step.
The rationale behind this staged pre-sintering plus staged pressing strategy is to gradually release thermal stresses and compaction stresses within the compact, avoiding the sharp shrinkage and cracking that would result from a single high-temperature, high-pressure step. The patent literature explicitly states that this method “can effectively prevent the target from cracking due to the hard and brittle nature of the raw materials, improve the yield of the target, and further enhance the density of the target.”
For applications requiring higher density, hot isostatic pressing (HIP) routes are employed. In one study, chromium powder and chromium-silicon alloy powder were used as raw materials, cold isostatically pressed, encapsulated, degassed, and then subjected to hot isostatic pressing at 1100–1300 °C and 120–150 MPa, yielding targets with relative density of 99.0%–99.7% and average grain sizes controlled in the range of 35–50 μm. Another patent route using CrSi₂ pre-alloyed powder and Cr powder as raw materials can likewise achieve targets with relative density >99%, with emphasis on grain size uniformity.
Regardless of the route employed, finished targets must be machined to specified dimensions and verified free of internal defects by ultrasonic inspection or density measurement before delivery. For planar or tubular targets used in large-area coating lines, the bonding quality between the target and backing plate—including bond coverage and thermal conductivity—is also a critical process step determining sputtering stability.
III. Performance Characteristics
The performance evaluation of Cr-Si targets ultimately rests on the behavior of the films they deposit, and film performance is jointly determined by target composition and microstructure.
In terms of electrical properties, the resistivity of Cr-Si films is continuously adjustable with chromium content. The introduction of chromium creates conductive pathways or silicide phases within the silicon-based film, transitioning it from a relatively semiconducting high-resistance state to a practical resistance range suitable for precision resistors. In thin-film resistor applications, the core metric is the controllability of the temperature coefficient of resistance (TCR). Through matching of target composition and post-deposition heat treatment, the TCR of Cr-Si films can be tuned to near zero or customized as needed, thereby maintaining resistance stability across the wide temperature range required by automotive electronics and industrial measurement.
In terms of optical properties, chromium content significantly affects the transmittance of oxide films obtained by reactive sputtering. Data from a study on silicon-chromium oxide films show: an oxide film deposited from a target containing 58 wt% Cr exhibited transmittance of approximately 81.2% at 550 nm after 29 passes (thickness 1593 Å); when chromium content was reduced to 25 wt%, transmittance reached 89.8% after 39 passes (thickness 2123 Å); and at only 10 wt% Cr, transmittance reached 92.8% after 16 passes (thickness 1044 Å). The trend is clear: the lower the chromium content, the better the transparency of the oxide film. When sputtered in a nitrogen atmosphere, chromium-containing films generally exhibit strong absorption characteristics, making them suitable for light-shielding or anti-reflection applications.
In terms of physical and chemical stability, the incorporation of chromium enhances the hardness and corrosion resistance of silicon-based films. Chromium oxides and nitrides possess high chemical inertness, making Cr-Si-based coatings more durable than pure silicon coatings in high-temperature or corrosive environments. The target material itself exhibits high melting point, good thermal conductivity, and chemical stability, meeting the requirements for use in high-temperature sputtering environments.
Post time: Nov-24-2026